Research Article
Wear Properties of TiC-Reinforced Co50 Composite Coatings from Room Temperature to High Temperature
Table 6
Wear weight losses of the samples in the friction-wear test at room temperature and 700°C.
| Condition | Sample | Wear weight loss (mg) | H13 steel | S0 | S1 | S2 |
| Room temperature | Coating | 27.8 | 23.9 | 19.6 | 18.0 | Cr12MoV | 40.6 | 4.3 | 8.8 | 14.3 |
| 700°C | Coating | 3.0 | 5.5 | 5.2 | 5.0 | Cr12MoV | 4989.7 | 65.1 | 273.0 | 360.5 |
|
|