Buckling eigenvalues of FE analysis.
| | Order | h = 4 | h = 3 | h = 2 | h = 1 |
| Delaminate area | 1 | 42.636 | 42.623 | 42.534 | 38.201 | 2 | 95.355 | 95.345 | 94.391 | 43.334 | 3 | 103.06 | 103.01 | 102.08 | 60.397 | 4 | 137.08 | 137.02 | 121.94 | 85.139 | 5 | 165.22 | 165.05 | 137.94 | 87.243 | 6 | 197.16 | 197.08 | 158.38 | 95.791 |
| Delaminate area | 1 | 41.226 | 41.153 | 41.070 | 18.191 | 2 | 88.140 | 88.092 | 64.774 | 28.951 | 3 | 91.639 | 91.162 | 88.945 | 40.451 | 4 | 129.28 | 120.32 | 91.391 | 40.729 | 5 | 143.57 | 129.92 | 105.68 | 42.803 | 6 | 176.95 | 148.75 | 126.07 | 53.590 |
| Delaminate area | 1 | 37.651 | 37.136 | 36.486 | 10.640 | 2 | 76.330 | 73.187 | 43.620 | 16.981 | 3 | 78.337 | 77.827 | 59.469 | 23.830 | 4 | 113.55 | 87.960 | 76.912 | 23.844 | 5 | 118.89 | 113.47 | 83.001 | 31.163 | 6 | 119.31 | 116.76 | 92.039 | 37.284 |
|
|