Research Article
Grain Growth of AZ31 Magnesium Alloy Based on Three-Dimensional Cellular Automata
Figure 10
The metallographic structure of the cross section at different temperatures. (a) Original grain structure before solution treatment. (b) After holding at 300°C for 12 h. (c) After holding at 380°C for 12 h. (d) After holding at 420°C for 12 h.
(a) |
(b) |
(c) |
(d) |