A Study on the Wear Characteristics of Al7075 with Changes in Surface Roughness and Ti Thin Film Deposition Time
Figure 1
Photograph of thin film thickness using SEM equipment: (a) 30′ sputtered specimen; (b) 60′ sputtered specimen; (c) 90′ sputtered specimen; (d) thin film low magnification photo.
(a) |
(b) |
(c) |
(d) |