Research Article
A Study on the Wear Characteristics of Al7075 with Changes in Surface Roughness and Ti Thin Film Deposition Time
Table 3
Deposition time according to surface roughness.
| | Surface roughness (sandpaper polishing number) | | #400 | #800 | #1200 | #Alumina (0.3 µm) |
| Deposition time (min) | 0′ | 1 | 2 | 3 | 4 | 30′ | 5 | 6 | 7 | 8 | 60′ | 9 | 10 | 11 | 12 | 90′ | 13 | 14 | 15 | 16 |
|
|