Research Article
Structural Behavior of Concrete Beams Containing Recycled Coarse Aggregates under Flexure
Table 1
Properties of the coarse aggregates.
| ā | Even-dry density (g/cm3) | SD (g/cm3) | Absorption (%) | SD (%) | Fineness modulus | Maximum diameter (mm) |
| Recycled coarse aggregate | 2.49 | 0.13 | 2.95 | 0.37 | 6.36 | 13 | Natural coarse aggregate | 2.62 | 0.17 | 0.57 | 0.11 | 6.55 | 25 |
|
|
SD: standard deviation.
|