Dielectric Relaxation Spectroscopy in Synthetic Rubber Polymers: Nitrile Butadiene Rubber and Ethylene Propylene Diene Monomer
Figure 9
(a) the glass transition temperature determined by DRS and (b) the glass transition temperature determined by DSC.