Microstructure and Properties of a 2.25Cr1Mo0.25V Heat-Resistant Steel Produced by Wire Arc Additive Manufacturing

Table 1

Chemical composition (wt%) of the 2.25Cr1Mo0.25V solid wire.

SampleCSiMnCrMoVNiFe

2.25Cr1Mo0.25V0.0980.1350.3982.371.000.2890.017Bal.