Research Article
Effects of Simulation-Guided Microwave Presintering Process on the Preparation and Final Properties of Pure Ceramic Rings: Lower Sintering Temperature and Higher Mechanical Properties
Figure 9
SEM images of four ceramic rings of group B obtained at different microwave sintering temperatures. (a) 1300°C, (b) 1350°C, (c) 1400°C, and (d) 1450°C.
(a) |
(b) |
(c) |
(d) |