Research Article
Study on the Parameter Optimization and Strength Mechanism of Coal Gangue Emulsified Asphalt Mixture
Table 6
Orthogonal test designs table.
| Level | Parameters | Parameter A | Parameter B | Parameter C | Coal gangue | Content of emulsified asphalt | Water consumption |
| 1 | 3% | 6.5% | 4% | 2 | 4% | 7% | 4.5% | 3 | 5% | 7.5% | 5% | 4 | 6% | 8% | 5.5% |
|
|