Research Article
Effect of Microarc Oxidation Treatment with Different Concentrations of MgSiF6 on Titanium-Porcelain Bonding Strength
Figure 1
SEM microphotographs of MAO coating: (a) control group, (b) 10 g/L MgSiF6 group, (c) 20 g/L MgSiF6 group, (d) 30 g/L MgSiF6 group, and (e) 40 g/L MgSiF6 group. Bar = 1 μm.
(a) |
(b) |
(c) |
(d) |
(e) |