Research Article

Effect of Microarc Oxidation Treatment with Different Concentrations of MgSiF6 on Titanium-Porcelain Bonding Strength

Figure 2

SEM microphotographs of the fracture surface of titanium specimens: (a) control group, (b) 10 g/L MgSiF6 group, (c) 20 g/L MgSiF6 group, (d) 30 g/L MgSiF6 group, and (e) 40 g/L MgSiF6 group. Bar = 100 μm. The residual porcelain is indicated by arrows.
(a)
(b)
(c)
(d)
(e)