Research Article
Effect of Microarc Oxidation Treatment with Different Concentrations of MgSiF6 on Titanium-Porcelain Bonding Strength
Figure 3
SEM microphotographs of titanium-porcelain interface: (a) control group, (b) 10 g/L MgSiF6 group, (c) 20 g/L MgSiF6 group, (d) 30 g/L MgSiF6 group, and (e) 40 g/L MgSiF6 group. Bar = 10 μm. The pores and cracks are indicated by arrows.
(a) |
(b) |
(c) |
(d) |
(e) |