Research Article
Effect of Microarc Oxidation Treatment with Different Concentrations of MgSiF6 on Titanium-Porcelain Bonding Strength
Table 1
Sintering condition of the porcelain.
| Porcelain | Starting temperature (°C) | Sintering temperature (°C) | Vacuum (MPa) | Sintering time (min) | Porcelain coating thickness (mm) |
| Bonding agent | 500 | 800 | 0.099 | 3 | 0.2 | Opaque | 500 | 780 | 0.099 | 3 | 0.2 | Dentin | 500 | 760 | 0.096 | 5 | 0.6 |
|
|