Research Article
Effect of Microarc Oxidation Treatment with Different Concentrations of MgSiF6 on Titanium-Porcelain Bonding Strength
Table 2
Effect of electrolyte concentrations on the Mao coating (wt%, n = 6).
| Groups | Ti | Si | O | F |
| 10 g/L MgSiF6 | 40.65 ± 0.60 | 8.91 ± 0.51 | 48.59 ± 0.27 | 1.86 ± 0.21 | 20 g/L MgSiF6 | 40.59 ± 0.92 | 3.16 ± 0.24 | 39.30 ± 1.19 | 16.95 ± 2.03 | 30 g/L MgSiF6 | 28.83 ± 0.94 | 1.87 ± 0.10 | 24.23 ± 0.74 | 45.07 ± 1.68 | 40 g/L MgSiF6 | 13.92 ± 0.44 | 0.76 ± 0.13 | 13.89 ± 0.32 | 71.43 ± 2.65 |
|
|
, compared to the control group. |