Research Article

Effect of Microarc Oxidation Treatment with Different Concentrations of MgSiF6 on Titanium-Porcelain Bonding Strength

Table 3

Bonding strength of different titanium-porcelain restorations (mean ± SD, n = 10).

GroupKBond strength (MPa)

10 g/L MgSiF64.738.18 ± 2.65
20 g/L MgSiF64.744.75 ± 2.21
30 g/L MgSiF64.731.44 ± 2.04
40 g/L MgSiF64.728.04 ± 2.59
Control group4.727.08 ± 3.16

, compared to the control group.