Research Article
Effect of Combining Fiber and Textile Reinforcement on the Flexural Behavior of UHPC Plates
Table 4
Main properties of the used UHPC and UHPFRC mixtures 28 days after casting.
| Used mixtures | Compression strength (MPa) | Splitting tensile strength (MPa) | Young’s modulus (GPa) | Maximum grain size (mm) | Fiber content (vol%) |
| UHPC | 166.3 | 7.9 | 44.7 | 0.4 | 0 | UHPFRC | 172.5 | 16.1 | 49.3 | 0.4 | 2 |
|
|