Research Article

Investigation of Stereometric and Fractal Patterns of Spin-Coated LuMnO3 Thin Films

Table 4

Fractal and parameters’ advanced fractal of LuMnO3 thin films.

ParameterUnitLuMnO650LuMnO750LuMnO850

FD(—)2.391 ± 0.0112.331 ± 0.0622.264 ± 0.020
HC(—)0.113 ± 0.0160.273 ± 0.0270.863 ± 0.013
ǀβǀ(—)5.33e−06 ± 3.34e−062.06e−06 ± 1.40e−066.97e−08 ± 4.84e−08
FS(—)0.522 ± 0.0020.512 ± 0.0130.510 ± 0.027
E(—)0.973 ± 0.0040.952 ± 0.0460.977 ± 0.014

denotes samples without significant difference, ANOVA One-Way and Tukey Test ().