Figure 3

SEM image of (a) Al 7075 [84], (b) Al 7075/10 wt.% of SiC (20–40 μm) [84], (c) Al 7075/15 wt.% of SiC (20–40 μm) [84], (d) Al 7075/15 wt.% of SiC (25 μm) [85], (e) Al 7075/15 wt.% of SiC (50 μm) [85], and (f) Al 7075/15 wt.% of SiC (75 μm) [85].
(a)
(b)
(c)
(d)
(e)
(f)