Advances in Materials Science and Engineering / 2023 / Article / Tab 5 / Review Article
A Systematic Review on the Mechanical, Tribological, and Corrosion Properties of Al 7075 Metal Matrix Composites Fabricated through Stir Casting Process Table 5 Fabrication methods for various Al-MMCs.
S. no. Ref. Matrix Fabrication method Properties studied 1 [34 ] 1060 Powder metallurgy Wear 2 [35 ] 1100 Accumulative roll bonding Elongation, microhardness, and TS 3 [36 ] Stir casting Yield strength, TS, and % elongation 4 [37 ] 2009 Powder metallurgy Corrosion 5 [38 ] 2011 Stir casting Wear 6 [39 ] 2014 Squeeze casting Wear and friction 7 [40 ] 2024 Squeeze casting Hardness and wear 8 [41 ] Stir casting Wear 9 [42 ] Pressure infiltration Bending strength 10 [43 ] Powder metallurgy Wear 11 [44 ] Vortex method and applied pressure Hardness and TS 12 [45 ] 2124 Powder metallurgy Fatigue behavior 13 [46 ] 2219 Liquid metallurgy Wear 14 [47 ] 2618 Squeeze casting Wear 15 [48 ] 5052 Pressure less infiltration TS 16 [49 ] 5059 Stir casting Hardness and wear 17 [50 ] 6061 Stir casting Hardness, ultimate TS, and wear 18 [51 ] Vacuum hot pressing TS 19 [52 ] 6063 Liquid metallurgy Wear 20 [53 ] 6351 Stir casting Wear 21 [54 ] 7005 Compo casting TS, hardness, and fracture 22 [55 ] 7055 Powder metallurgy Fatigue behavior 23 [56 ] 7075 Stir casting Ultimate TS and hardness 24 [57 ] Liquid casting TS, hardness, and wear 25 [58 ] 8090 Spray deposition Wear