Deformation of SS 304 LN during Scratch Test and Influence on Evolution of Coefficient of Friction

Figure 1

(a) The ratio of residual depth to penetration depth for progressive load ranging between 1 N to 15 N at three different values of scratch speed , 3, and 27 mm/min, (b) frictional force with progressive normal force acting on to the material SS AISI 304, and (c) the evolution of coefficient of friction for scratch speed , 3, and 27 mm/min.
648075.fig.001a
(a)
648075.fig.001b
(b)
648075.fig.001c
(c)